APTIV® 2100 Series Film 125µm

Alternative and trade names
APTIV® 2100 Series Film 125µm
Want to keep this datasheet? Save it now in your required format

Description

APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 2100 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format.


Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users. APTIV 2100 series provides a higher modulus over the APTIV 2000 series amorphous films. This grade is tailored towards thermoforming of thin wall parts with higher modulus, such as speaker diaphragms.


Please note - APTIV 2100 will crystallise if taken above the Tg [143°C (289°F)] in either secondary processes or end use application. The crystallisation is not reversible back to the amorphous phase without remelting the material. Consideration of the temperature range during processing and end use application needs to be included if selecting APTIV 2100.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Thickness

0.13 mm

Show Material materials with Thickness of 0.13 mm

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3 GPa

Show Material materials with Elastic modulus of 3 GPa

ISO 527

Elastic modulus, transverse

23.0 °C

3 GPa

Show Material materials with Elastic modulus, transverse of 3 GPa

ISO 527

Elongation

23.0 °C

150 %

Show Material materials with Elongation of 150 %

ISO 527

Elongation, transverse

23.0 °C

150 %

Show Material materials with Elongation, transverse of 150 %

ISO 527

Tensile strength

23.0 °C

100 MPa

Show Material materials with Tensile strength of 100 MPa

ISO 527

Tensile strength, transverse

23.0 °C

80 MPa

Show Material materials with Tensile strength, transverse of 80 MPa

ISO 527

Thermal

PropertyValue

Glass transition temperature

143 °C

Show Material materials with Glass transition temperature of 143 °C

Technological properties

Property
Application areas

Electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts

Certifications

APTIV 2100 film is approved for food contact Use: APTIV 2100 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2100 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2100 film complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2100 film is inherently halogen-free in accordance with IEC61249-2-21.

Other

The key features are: High heat resistance, excellent flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable, excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties and barrier properties, high purity, lightweight, recyclable, easy to process.

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.