Polyaramid Honeycomb B

Want to keep this datasheet? Save it now in your required format

Description

The product is an aramid polymer with a particularly stable molecular structure . It is obtained from different forms of aramid polymer.


Non-metallic honeycombs are manufactured from high temperature resistant aramid paper formed into a honeycomb structure and coated with a phenolic resin. The combination of aramid paper and phenolic resin gives commercial and aero grade of honeycomb with superior strength, toughness and chemical resistance.


The honeycomb cell shapes are normally hexagonal for optimum mechanical properties. It can also be over-expanded to produce a rectangular cell shape and provide improved drapeability for the production of curved parts.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Compressive modulus

23.0 °C

75 MPa

Show Material materials with Compressive modulus of 75 MPa

Compressive strength

23.0 °C

1.2 MPa

Show Material materials with Compressive strength of 1.2 MPa

Shear modulus, L direction

23.0 °C

29 MPa

Show Material materials with Shear modulus, L direction of 29 MPa

Shear modulus, W direction

23.0 °C

19 MPa

Show Material materials with Shear modulus, W direction of 19 MPa

Shear strength, L direction

23.0 °C

0.7 MPa

Show Material materials with Shear strength, L direction of 0.7 MPa

Shear strength, W direction

23.0 °C

0.4 MPa

Show Material materials with Shear strength, W direction of 0.4 MPa

Technological properties

Property
Application areas

Aerospace applications: Helicopter blades, fairings, interior panels, flooring, control surfaces, flaps, engine nacelles; HexWeb A1 honeycomb is qualified to all major aerospace specifications. Industrial applications: Marine and ground transportation, interior panels, flooring, bulkheads, hatches; racing boat shells; high performance car chassis and body panels; precision optical equipment; desiccant and filtration systems; radar reflectors, covers and emitters.

Other

The key features are: Outstanding resistance to corrosive attack by chemicals, high mechanical strength at low densities, fire retardant and self-extinguishing, excellent resistance to impact damage and moisture, low smoke and toxic gas emission, highly resistant to fungal growth, good dielectric properties, transparent radio and radar waves, low thermal conductivity