General
Property | Value |
---|---|
Density | 0.85 g/cm³ Show Material materials with Density of 0.85 g/cm³ |
Molar mass | 12000.0 g/mol Show Material materials with Molar mass of 12000.0 g/mol |
Thermal
Optical
Property | Value |
---|---|
Refractive index | 1.4735 [-] Show Material materials with Refractive index of 1.4735 [-] |
Technological properties
Property | ||
---|---|---|
Other | Soluble in: Chlorinated hydrocarbons, diethyl ether, hydrocarbons, isoamyl acetate, toluene; Insoluble in more polar organic solvents with small hydrocarbon groups even at elevated temperatures. |