General
Mechanical
Property | Value |
---|---|
Elongation | 45.0 % Show Material materials with Elongation of 45.0 % |
Flexural modulus | 0.59 GPa Show Material materials with Flexural modulus of 0.59 GPa |
Flexural strength | 14.0 MPa Show Material materials with Flexural strength of 14.0 MPa |
Hardness, Shore D | 66.0 [-] Show Material materials with Hardness, Shore D of 66.0 [-] |
Impact strength, Izod unnotched, ASTM | 37.0 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 37.0 J/m |
Tensile strength | 13 MPa Show Material materials with Tensile strength of 13 MPa |
Thermal
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 50 g/10min Show Material materials with Melt mass-flow rate of 50 g/10min | 175°C/5 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Molded products, bowl, trays, containers, cup, tumbler, disposable cutleries (<120°C) | |
Certifications | Food Contact: Halal | |
Processing methods | 1. Clean extruder with general purpose polyethylene or polypropylene. 2. Vacuum out hopper system to avoid contamination and make sure that the humidity of the air is below 40°C at dew point. 3. Introduce ICBP Bio Resin in to the extruder at the operating conditions used in the first step. 4. Once ICBP Bio Resin has been purged, reduce barrel temperatures to desired set points. 5. At shutdown, purge machine with PE or PP. |