Properties

General

PropertyValue

Bio-based content

100 %

Show Material materials with Bio-based content of 100 %

Density

1.3 g/cm³

Show Material materials with Density of 1.3 g/cm³

Mechanical

PropertyValue

Elongation

30.0 %

Show Material materials with Elongation of 30.0 %

Flexural modulus

2.0 GPa

Show Material materials with Flexural modulus of 2.0 GPa

Flexural strength

65.0 MPa

Show Material materials with Flexural strength of 65.0 MPa

Hardness, Shore D

70.0 [-]

Show Material materials with Hardness, Shore D of 70.0 [-]

Impact strength, Izod unnotched, ASTM

20.0 J/m

Show Material materials with Impact strength, Izod unnotched, ASTM of 20.0 J/m

Tensile strength

40 MPa

Show Material materials with Tensile strength of 40 MPa

Thermal

PropertyValue

Decomposition heat

220.0 J/g

Show Material materials with Decomposition heat of 220.0 J/g

Melting point

140 °C

Show Material materials with Melting point of 140 °C

Rheological Properties

PropertyValueComment

Melt mass-flow rate

8 g/10min

Show Material materials with Melt mass-flow rate of 8 g/10min

160°C/2.16kg

Technological properties

Property
Application areas

Straw, tube

Certifications

Food Contact: Halal

Processing methods