General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 20.0 °C | 0.91 g/cm³ Show Material materials with Density of 0.91 g/cm³ | |
Film yield | 20.0 °C | 22.89 - 36.63 m²/kg Show Material materials with Film yield of 22.89 - 36.63 m²/kg | |
Shrinkage | 120.0 °C | 4 % Show Material materials with Shrinkage of 4 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Shrinkage, transverse | 120.0 °C | 2 % Show Material materials with Shrinkage, transverse of 2 % | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Surface density | 20.0 °C | 2.73E-3 - 4.37E-3 g/cm² Show Material materials with Surface density of 2.73E-3 - 4.37E-3 g/cm² |
Dimension
Property | Value |
---|---|
Thickness | 0.03 - 0.05 mm Show Material materials with Thickness of 0.03 - 0.05 mm |
Dimensions | Available thicknesses: 30, 35, 40, 48µm. |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elongation | 20.0 °C | 200 % Show Material materials with Elongation of 200 % | GOST 14236, ISO 527, ASTM D882 |
Elongation, transverse | 20.0 °C | 70 % Show Material materials with Elongation, transverse of 70 % | GOST 14236, ISO 527, ASTM D882 |
Tensile strength | 20.0 °C | 140 MPa Show Material materials with Tensile strength of 140 MPa | GOST 14236, ISO 527, ASTM D882 |
Tensile strength, transverse | 20.0 °C | 280 MPa Show Material materials with Tensile strength, transverse of 280 MPa | GOST 14236, ISO 527, ASTM D882 |
Optical
Property | Value | Comment |
---|---|---|
Haze | 2 % Show Material materials with Haze of 2 % | GOST 15875, ISO 14782, ASTM D 1003 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality solvent based rotogravure and flexographic printing, for production of fully wrapped labels for bottles, for labeling with cold and hot melt glue, solvent based and solvent free lamination with polyurethane adhesives (if necessary). | |
Friction | Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | LGBA BOPP films comprise: A treated side of modified copolymer skin layer, a transparent biaxially oriented polypropylene; a glossy, none treated, Non-heat-sealable polypropylene skin layer with standard coefficient of friction. | |
Processing history | Treatment level: 38 mN/m (ISO 8296, ASTM D 2578). |