Description

White Pearl microporous BOPP film for fully wrapped labeling of bottles for cold and hot melt glue application while labeling with good gloss and ink adhesion. The main advantages are: High adhesion of solvent based inks: flexo and rotogravure for direct printing; both side glossy film; good opacity and whiteness; contains slip, antistatic and antiblock additives; contains mineral fillers such as calcium carbonate and titanium dioxide; low coefficient of friction, stable in time; without coating or primer.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.68 g/cm³

Show Material materials with Density of 0.68 g/cm³

Film yield

20.0 °C

31.29 - 42.02 m²/kg

Show Material materials with Film yield of 31.29 - 42.02 m²/kg

Shrinkage

120.0 °C

4 %

Show Material materials with Shrinkage of 4 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 %

Show Material materials with Shrinkage, transverse of 2 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

2.38E-3 - 3.2E-3 g/cm²

Show Material materials with Surface density of 2.38E-3 - 3.2E-3 g/cm²

Dimension

PropertyValue

Thickness

0.04 - 0.05 mm

Show Material materials with Thickness of 0.04 - 0.05 mm

Dimensions

Available thicknesses: 35, 38, 47µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 %

Show Material materials with Elongation of 200 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 %

Show Material materials with Elongation, transverse of 70 %

GOST 14236, ISO 527, ASTM D882

Tensile strength

20.0 °C

80 MPa

Show Material materials with Tensile strength of 80 MPa

GOST 14236, ISO 527, ASTM D882

Tensile strength, transverse

20.0 °C

150 MPa

Show Material materials with Tensile strength, transverse of 150 MPa

GOST 14236, ISO 527, ASTM D882

Optical

PropertyValueComment

Luminous transmittance

20 - 30 [-]

Show Material materials with Luminous transmittance of 20 - 30 [-]

GOST 15875, ISO 14782, ASTM D 1003

Technological properties

Property
Application areas

High quality solvent rotogravure and flexographic direct printing, for production of fully wrapped labels for bottles, for labeling with cold and hot melt glue.

Friction

Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894).

Other

LOBA BOPP films comprise: A modified copolymer corona treated skin layer, a white opaque oriented polypropylene tie layer, a white pearl cavitated core layer of oriented polypropylene, an oriented polypropylene tie layer, a glossy non-heat-sealable, non treated skin layer with standard coefficient of friction.

Processing history

Treatment level: 38 mN/m (ISO 8296, ASTM D 2578).