PMD.M BOPP (Biaxially Oriented Polypropylene) Metallized Film

Want to keep this datasheet? Save it now in your required format

Description

Non-heat-sealable metallized BOPP film for the production of decorative packaging. With increased coefficient of friction. For printing and lamination and for decorative packaging. The main advantages are: Standard barrier properties of metallized films; contains antiblock additives; mechanical properties are good; high adhesion of the aluminum layer; intended for contact with food; without coating or primer.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

Film yield

20.0 °C

27.5 - 54.9 m²/kg

Show Material materials with Film yield of 27.5 - 54.9 m²/kg

Shrinkage

120.0 °C

4 %

Show Material materials with Shrinkage of 4 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 %

Show Material materials with Shrinkage, transverse of 2 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

1.82E-3 - 3.64E-3 g/cm²

Show Material materials with Surface density of 1.82E-3 - 3.64E-3 g/cm²

Dimension

PropertyValue

Thickness

0.02 - 0.04 mm

Show Material materials with Thickness of 0.02 - 0.04 mm

Dimensions

Available thicknesses: 20, 25, 30, 35, 40µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 %

Show Material materials with Elongation of 200 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 %

Show Material materials with Elongation, transverse of 70 %

GOST 14236, ISO 527, ASTM D882

Tensile strength

20.0 °C

140 MPa

Show Material materials with Tensile strength of 140 MPa

GOST 14236, ISO 527, ASTM D882

Tensile strength, transverse

20.0 °C

280 MPa

Show Material materials with Tensile strength, transverse of 280 MPa

GOST 14236, ISO 527, ASTM D882

Technological properties

Property
Application areas

High quality rotogravure and flexographic solvent based printing; for lamination with solvent based or solventless polyurethane adhesives; production of decorative packaging for flowers, gift wrap and etc.; heat sealing by string is possible; lamination with films, paper and cardboard.

Friction

Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894).

Other

PMD.M BOPP films comprise: An aluminum layer, a treated modified copolymer layer for aluminum adhesion, a transparent oriented polypropylene core layer, a non-heat-sealable skin layer with high coefficient of friction, without treatment.

Processing history

Treatment level: 36 mN/m (ISO 8296, ASTM D 2578).