General
Property | Value | Temperature | Comment |
---|---|---|---|
Density | 0.91 g/cm³ Show Material materials with Density of 0.91 g/cm³ at 20.0 °C | 20.0 °C | |
Film yield | 27.5 - 54.9 m²/kg Show Material materials with Film yield of 27.5 - 54.9 m²/kg at 20.0 °C | 20.0 °C | |
Shrinkage | 4 % Show Material materials with Shrinkage of 4 % at 120.0 °C | 120.0 °C | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Shrinkage, transverse | 2 % Show Material materials with Shrinkage, transverse of 2 % at 120.0 °C | 120.0 °C | GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min) |
Surface density | 1.82E-3 - 3.64E-3 g/cm² Show Material materials with Surface density of 1.82E-3 - 3.64E-3 g/cm² at 20.0 °C | 20.0 °C |
Dimension
Property | Value |
---|---|
Dimensions | Available thicknesses: 20, 25, 30, 35, 40µm. |
Thickness | 0.02 - 0.04 mm Show Material materials with Thickness of 0.02 - 0.04 mm |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 200 % Show Material materials with Elongation of 200 % at 20.0 °C | 20.0 °C | GOST 14236, ISO 527, ASTM D882 |
Elongation, transverse | 70 % Show Material materials with Elongation, transverse of 70 % at 20.0 °C | 20.0 °C | GOST 14236, ISO 527, ASTM D882 |
Tensile strength | 140 MPa Show Material materials with Tensile strength of 140 MPa at 20.0 °C | 20.0 °C | GOST 14236, ISO 527, ASTM D882 |
Tensile strength, transverse | 280 MPa Show Material materials with Tensile strength, transverse of 280 MPa at 20.0 °C | 20.0 °C | GOST 14236, ISO 527, ASTM D882 |
Technological properties
Property | ||
---|---|---|
Application areas | High quality rotogravure and flexographic solvent based printing; for lamination with solvent based or solventless polyurethane adhesives; production of decorative packaging for flowers, gift wrap and etc.; heat sealing by string is possible; lamination with films, paper and cardboard. | |
Friction | Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894). | |
Other | PMD.M BOPP films comprise: An aluminum layer, a treated modified copolymer layer for aluminum adhesion, a transparent oriented polypropylene core layer, a non-heat-sealable skin layer with high coefficient of friction, without treatment. | |
Processing history | Treatment level: 36 mN/m (ISO 8296, ASTM D 2578). |