PMP.M BOPP (Biaxially Oriented Polypropylene) Metallized Film

Want to keep this datasheet? Save it now in your required format

Description

Metallized non-heat-sealable both side treated BOPP film with standard coefficient of friction for both side printing and lamination. The main advantages are: Both sides (T, UT) activated film; standard barrier properties of metallized films; standard coefficient of friction; mechanical properties and aluminum adhesian are good; contains no migratory antiblock and slip additives; intended for contact with food; without coating or primer.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

Film yield

20.0 °C

27.5 - 54.9 m²/kg

Show Material materials with Film yield of 27.5 - 54.9 m²/kg

Shrinkage

120.0 °C

4 %

Show Material materials with Shrinkage of 4 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 %

Show Material materials with Shrinkage, transverse of 2 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

1.82E-3 - 3.64E-3 g/cm²

Show Material materials with Surface density of 1.82E-3 - 3.64E-3 g/cm²

Dimension

PropertyValue

Thickness

0.02 - 0.04 mm

Show Material materials with Thickness of 0.02 - 0.04 mm

Dimensions

Available thicknesses: 20, 25, 30, 35, 40µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 %

Show Material materials with Elongation of 200 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 %

Show Material materials with Elongation, transverse of 70 %

GOST 14236, ISO 527, ASTM D883

Tensile strength

20.0 °C

140 MPa

Show Material materials with Tensile strength of 140 MPa

GOST 14236, ISO 527, ASTM D883

Tensile strength, transverse

20.0 °C

250 MPa

Show Material materials with Tensile strength, transverse of 250 MPa

GOST 14236, ISO 527, ASTM D883

Technological properties

Property
Application areas

Rotogravure and flexographic solvent based one or both side printing; for both side lamination with solvent based or solventless polyurethane adhesives; lamination with films, paper and cardboard, as well as in the center of the triplex in flexible packaging; for the production of labels with both side printed design.

Friction

Kinetic coefficient of friction µ= 0.2-0.4 (GOST 27492, ISO 8295, ASTM D 1894).

Other

PMP.M BOPP Films comprise: An aluminum layer, a treated modified copolymer layer for aluminum adhesion, a transparent oriented polypropylene core layer, a treated non-heat-sealable skin layer with standard coefficient of friction.

Processing history

Treatment level: 36-38 mN/m (ISO 8296, ASTM D 2578).