HGHW BOPP (Biaxially Oriented Polypropylene) Transparent Film

Want to keep this datasheet? Save it now in your required format

Description

Transparent heat sealable BOPP film with a wide temperature sealing range, and low coefficient of friction for high speed packaging machines for high quality rotogravure and flexographic printing. The main advantages are: A very wide range of heat sealing; sufficiently low coefficient of friction, including the heated surfaces for high-speed packaging machines; contains slip-antistatic and antiblocking additives; excellent optical properties; good mechanical properties; intended for contact with food; permanent coefficient of friction, even after printing and lamination; without coatings and primers.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

Film yield

20.0 °C

22.89 - 73.26 m²/kg

Show Material materials with Film yield of 22.89 - 73.26 m²/kg

Shrinkage

120.0 °C

4 - 5 %

Show Material materials with Shrinkage of 4 - 5 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 - 3 %

Show Material materials with Shrinkage, transverse of 2 - 3 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

1.36E-3 - 4.37E-3 g/cm²

Show Material materials with Surface density of 1.36E-3 - 4.37E-3 g/cm²

Dimension

PropertyValue

Thickness

0.02 - 0.05 mm

Show Material materials with Thickness of 0.02 - 0.05 mm

Dimensions

Available thicknesses: 15, 18, 20, 25, 30, 35, 40, 48µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 - 220 %

Show Material materials with Elongation of 200 - 220 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 - 80 %

Show Material materials with Elongation, transverse of 70 - 80 %

GOST 14236, ISO 527, ASTM D882

Tensile strength

20.0 °C

130 - 140 MPa

Show Material materials with Tensile strength of 130 - 140 MPa

GOST 14236, ISO 527, ASTM D882

Tensile strength, transverse

20.0 °C

230 - 250 MPa

Show Material materials with Tensile strength, transverse of 230 - 250 MPa

GOST 14236, ISO 527, ASTM D882

Optical

PropertyValueComment

Haze

2.5 - 3.2 %

Show Material materials with Haze of 2.5 - 3.2 %

GOST 15875, ISO 14782, ASTM D 1003

Technological properties

Property
Application areas

High quality solvent based rotogravure and flexographic printing; solvent based and solvent free lamination with polyurethane adhesives; manufacture of flexible packaging for food products; for high speed vertical VFFS and horizontal HFFS packaging machines; for heatsealing by UT / UT (fin seam) and UT / T (overlap) film sides; for applications requiring temperature decrease or increase the speed of heat sealing; not for corona treatment of UT side and not for cold seal coating of UT side.

Friction

Kinetic coefficient of friction µ= 0.1-0.35 (GOST 27492, ISO 8295, ASTM D 1894).

Other

HGHW BOPP film: a treated modified heat sealable copolymer skin layer, a transparent oriented polypropylene core layer, a heat sealable, non treated skin layer with very low seal intention temperature and standard coefficient of friction.

Processing history

Treatment level: 36 mN/m (ISO 8296, ASTM D 2578).