Description

Transparent release BOPP film for high quality rotogravure and flexographic printing and lamination; for the production of flexible packaging with frame cold seal glue. The main advantages are: UT side has a release properties to the latex cold seal glue; high optical: transparency and gloss and high physical and mechanical properties; low coefficient of friction, including hot surfaces, specially for HFFS machines; contains antistatic, slip-antiblocking and release additives; intended for contact with food; chemically resistant to oils, fats and chemicals.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

Film yield

20.0 °C

31.4 - 73.26 m²/kg

Show Material materials with Film yield of 31.4 - 73.26 m²/kg

Shrinkage

120.0 °C

4 - 5 %

Show Material materials with Shrinkage of 4 - 5 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Shrinkage, transverse

120.0 °C

2 %

Show Material materials with Shrinkage, transverse of 2 %

GOST 18616, ISO 11501, ASTM D1204 (Thermal shrinkage at 120˚C, 5 min)

Surface density

20.0 °C

1.36E-3 - 3.18E-3 g/cm²

Show Material materials with Surface density of 1.36E-3 - 3.18E-3 g/cm²

Dimension

PropertyValue

Thickness

0.02 - 0.04 mm

Show Material materials with Thickness of 0.02 - 0.04 mm

Dimensions

Available thicknesses: 15, 20, 25, 30, 35µm.

Mechanical

PropertyTemperatureValueComment

Elongation

20.0 °C

200 %

Show Material materials with Elongation of 200 %

GOST 14236, ISO 527, ASTM D882

Elongation, transverse

20.0 °C

70 %

Show Material materials with Elongation, transverse of 70 %

GOST 14236, ISO 527, ASTM D882

Tensile strength

20.0 °C

140 - 150 MPa

Show Material materials with Tensile strength of 140 - 150 MPa

GOST 14236, ISO 527, ASTM D882

Tensile strength, transverse

20.0 °C

250 MPa

Show Material materials with Tensile strength, transverse of 250 MPa

GOST 14236, ISO 527, ASTM D882

Optical

PropertyValueComment

Haze

2 %

Show Material materials with Haze of 2 %

GOST 15875, ISO 14782, ASTM D 1003

Technological properties

Property
Application areas

High quality rotogravure and flexographic solvent printing; solvent or solventless polyurethane laminating adhesives; for the production of flexible packaging (typically duplex) with frame cold seal glue.

Friction

Kinetic coefficient of friction µ= 0.1-0.35 (GOST 27492, ISO 8295, ASTM D 1894).

Other

PGR BOPP films comprise: A treated modified copolymer skin layer, a transparent oriented polypropylene core layer, a non-heat-sealable, untreated release skin layer with low coefficient of friction.

Processing history

Treatment level: 38 mN/m (ISO 8296, ASTM D 2578).