Amorphous Polyethylene terephthalate (APET) with food contact approval.

Properties

General

Density ρ

1.33 - 1.35 g/cm³ at 20 °C

Mechanical

Elastic modulus E

2.1 - 2.4 GPa at 20 °C

Elongation A

50 - 300 % at 20 °C

Impact strength, Charpy notched Ivnot

1 - 10 kJ/m² at 20 °C

Impact strength, Charpy unnotched Iunnot

no break

Max allowed stress σmax

55 MPa at 20 °C

at 4% strain

Thermal

Coefficient of thermal expansion α

7E-5 - 8E-5 1/K at 20 °C

Flammability

UL 94 HB

Max service temperature, long Tmaxlong

60 °C

Specific heat capacity cp

1050 J/(kg·K) at 20 °C

Thermal conductivity λ

0.2 - 0.24 W/(m·K) at 20 °C

Electrical

Dielectric constant εr

3.2 - 3.6 [-] at 20 °C

Electrical resistivity ρel

1.00E+13 Ω·m at 20 °C

Optical

Transparency

yes

Technological properties

Application areas

Bottles, refrigerators, food packaging

Fillers

Unfilled, no additives.

Processing methods

Injection molding, blow molding, extrusion

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.