General
Property | Value |
---|---|
Density | 0.93 - 0.94 g/cm³ Show Material materials with Density of 0.93 - 0.94 g/cm³ |
Mechanical
Property | Value |
---|---|
Elastic modulus | 0.03 - 0.1 GPa Show Material materials with Elastic modulus of 0.03 - 0.1 GPa |
Elongation | 100.0 - 900.0 % Show Material materials with Elongation of 100.0 - 900.0 % |
Impact strength, Charpy notched | no break |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00025 1/K Show Material materials with Coefficient of thermal expansion of 0.00025 1/K |
Melting point | 90.0 - 110.0 °C Show Material materials with Melting point of 90.0 - 110.0 °C |
Specific heat capacity | 2300 J/(kg·K) Show Material materials with Specific heat capacity of 2300 J/(kg·K) |
Thermal conductivity | 0.2 - 0.35 W/(m·K) Show Material materials with Thermal conductivity of 0.2 - 0.35 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.5 [-] Show Material materials with Dielectric constant of 2.5 [-] |
3 [-] Show Material materials with Dielectric constant of 3 [-] | |
Electrical resistivity | 100000000000000 Ω·m Show Material materials with Electrical resistivity of 100000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Flexible pipes, cable coating, gaskets, anesthesia masks, green house films | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming, coating |