General
Property | Value |
---|---|
Density | 1.03 - 1.07 g/cm³ Show Material materials with Density of 1.03 - 1.07 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 1.8 - 3.0 GPa Show Material materials with Elastic modulus of 1.8 - 3.0 GPa | |
Elongation | 2.0 - 60.0 % Show Material materials with Elongation of 2.0 - 60.0 % | |
Impact strength, Charpy notched | 2.0 - 24.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 2.0 - 24.0 kJ/m² | |
Impact strength, Charpy unnotched | 10 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 10 kJ/m² | |
Tensile strength | 30.0 - 65.0 MPa Show Material materials with Tensile strength of 30.0 - 65.0 MPa | at 2-6% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 8e-05 - 0.0001 1/K Show Material materials with Coefficient of thermal expansion of 8e-05 - 0.0001 1/K |
Specific heat capacity | 1300 J/(kg·K) Show Material materials with Specific heat capacity of 1300 J/(kg·K) |
Thermal conductivity | 0.13 - 0.18 W/(m·K) Show Material materials with Thermal conductivity of 0.13 - 0.18 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.8 [-] Show Material materials with Dielectric constant of 2.8 [-] |
3.1 [-] Show Material materials with Dielectric constant of 3.1 [-] | |
Electrical resistivity | 100000000000.0 - 10000000000000.0 Ω·m Show Material materials with Electrical resistivity of 100000000000.0 - 10000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Electrical housing, siphon traps, inhalation equipment, Lego | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |