General
Property | Value |
---|---|
Density | 1.04 - 1.07 g/cm³ Show Material materials with Density of 1.04 - 1.07 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 2.0 - 2.9 GPa Show Material materials with Elastic modulus of 2.0 - 2.9 GPa | |
Elongation | 10.0 - 70.0 % Show Material materials with Elongation of 10.0 - 70.0 % | |
Impact strength, Charpy notched | 10.0 - 40.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 10.0 - 40.0 kJ/m² | |
Impact strength, Charpy unnotched | 150 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 150 kJ/m² | |
Tensile strength | 40.0 - 55.0 MPa Show Material materials with Tensile strength of 40.0 - 55.0 MPa | at 2-6% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 8.5e-05 - 9.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 8.5e-05 - 9.5e-05 1/K |
Specific heat capacity | 1300 J/(kg·K) Show Material materials with Specific heat capacity of 1300 J/(kg·K) |
Thermal conductivity | 0.16 - 0.21 W/(m·K) Show Material materials with Thermal conductivity of 0.16 - 0.21 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 3.3 [-] Show Material materials with Dielectric constant of 3.3 [-] |
4 [-] Show Material materials with Dielectric constant of 4 [-] | |
Electrical resistivity | 1000000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 1000000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Housing microwaves, housing lawnmowers, radiator grills, surfboard shells | |
Processing methods | Injection molding, extrusion, thermoforming |