General
Property | Value |
---|---|
Density | 2.12 - 2.18 g/cm³ Show Material materials with Density of 2.12 - 2.18 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 0.4 - 0.7 GPa Show Material materials with Elastic modulus of 0.4 - 0.7 GPa | ||
Elongation | 250.0 - 330.0 % Show Material materials with Elongation of 250.0 - 330.0 % | ||
Tensile strength | 20.0 - 34.0 MPa Show Material materials with Tensile strength of 20.0 - 34.0 MPa | at 250-330% strain | |
Impact strength, Charpy notched | no break | ||
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 8e-05 - 0.00012 1/K Show Material materials with Coefficient of thermal expansion of 8e-05 - 0.00012 1/K |
Melting point | 255.0 - 285.0 °C Show Material materials with Melting point of 255.0 - 285.0 °C |
Specific heat capacity | 1120 J/(kg·K) Show Material materials with Specific heat capacity of 1120 J/(kg·K) |
Thermal conductivity | 0.25 W/(m·K) Show Material materials with Thermal conductivity of 0.25 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 2 [-] Show Material materials with Dielectric constant of 2 [-] |
2.15 [-] Show Material materials with Dielectric constant of 2.15 [-] | |
Electrical resistivity | 1000000000000000000 Ω·m Show Material materials with Electrical resistivity of 1000000000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Telecommunication cable jacketing, packaging films, heat-sealing adhesives | |
Processing methods | Injection molding, extrusion, compression molding |