General
Property | Value |
---|---|
Density | 1.17 - 1.19 g/cm³ Show Material materials with Density of 1.17 - 1.19 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 3.1 - 3.3 GPa Show Material materials with Elastic modulus of 3.1 - 3.3 GPa | |
Elongation | 2.0 - 10.0 % Show Material materials with Elongation of 2.0 - 10.0 % | |
Impact strength, Charpy notched | 1.2 - 2.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 1.2 - 2.0 kJ/m² | |
Impact strength, Charpy unnotched | 11 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 11 kJ/m² | |
22 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 22 kJ/m² | ||
Tensile strength | 30.0 - 80.0 MPa Show Material materials with Tensile strength of 30.0 - 80.0 MPa | at 2-10% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 6e-05 - 0.00012 1/K Show Material materials with Coefficient of thermal expansion of 6e-05 - 0.00012 1/K |
Specific heat capacity | 1470 J/(kg·K) Show Material materials with Specific heat capacity of 1470 J/(kg·K) |
Thermal conductivity | 0.18 - 0.19 W/(m·K) Show Material materials with Thermal conductivity of 0.18 - 0.19 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.7 [-] Show Material materials with Dielectric constant of 2.7 [-] |
3.7 [-] Show Material materials with Dielectric constant of 3.7 [-] | |
Electrical resistivity | 10000000000000 Ω·m Show Material materials with Electrical resistivity of 10000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Light guides, glasses, lenses, solar technology, optical data storage | |
Processing methods | Injection molding, extrusion, thermoforming |