The material: 'Polysulphone (PSU) Granules (SU346310)' you were looking for has been superseded by the one below.

Polysulfone (PSU)

Alternative and trade names
Udel®, Ultrason®
Want to keep this datasheet? Save it now in your required format

Description

It keeps stiffness and dimensional stability even when used at very high temperatures. It is used for molding high-quality engineering parts and highly stressed mass-produced articles. It is a rigid, high-strength, semi-tough, transparent plastic that offers higher heat resistance and better hydrolytic stability than polycarbonate. It retains its good mechanical properties when exposed to steam and other sterilization techniques.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.24 - 1.25 g/cm³

Show Material materials with Density of 1.24 - 1.25 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

2.5 - 2.8 GPa

Show Material materials with Elastic modulus of 2.5 - 2.8 GPa

Elongation

25.0 - 30.0 %

Show Material materials with Elongation of 25.0 - 30.0 %

Impact strength, Charpy notched

3.5 - 7.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 3.5 - 7.0 kJ/m²

Tensile strength

70.0 - 90.0 MPa

Show Material materials with Tensile strength of 70.0 - 90.0 MPa

at 6-22% strain

Impact strength, Charpy unnotched

no break

Thermal

PropertyValue

Coefficient of thermal expansion

5.5e-05 - 6e-05 1/K

Show Material materials with Coefficient of thermal expansion of 5.5e-05 - 6e-05 1/K

Specific heat capacity

1300 J/(kg·K)

Show Material materials with Specific heat capacity of 1300 J/(kg·K)

Thermal conductivity

0.15 - 0.28 W/(m·K)

Show Material materials with Thermal conductivity of 0.15 - 0.28 W/(m·K)

Flammability

UL 94 HB-V1

Electrical

PropertyValue

Dielectric constant

3 [-]

Show Material materials with Dielectric constant of 3 [-]

3.2 [-]

Show Material materials with Dielectric constant of 3.2 [-]

Electrical resistivity

10000000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000000 Ω·m

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

Mouth guards, switch latches, fuseholders, breaker covers, dental x-ray holders

Processing methods

Injection molding, blow molding, extrusion, thermoforming