General
Property | Value |
---|---|
Density | 1.3 - 1.35 g/cm³ Show Material materials with Density of 1.3 - 1.35 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 3.5 - 4.1 GPa Show Material materials with Elastic modulus of 3.5 - 4.1 GPa | ||
Elongation | 15.0 - 50.0 % Show Material materials with Elongation of 15.0 - 50.0 % | ||
Impact strength, Charpy notched | 4.0 - 10.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 4.0 - 10.0 kJ/m² | ||
Tensile strength | 90.0 - 120.0 MPa Show Material materials with Tensile strength of 90.0 - 120.0 MPa | at 5-7% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 4.5e-05 - 6e-05 1/K Show Material materials with Coefficient of thermal expansion of 4.5e-05 - 6e-05 1/K |
Melting point | 340.0 - 345.0 °C Show Material materials with Melting point of 340.0 - 345.0 °C |
Specific heat capacity | 2100.0 - 2200.0 J/(kg·K) Show Material materials with Specific heat capacity of 2100.0 - 2200.0 J/(kg·K) |
Thermal conductivity | 0.25 - 0.29 W/(m·K) Show Material materials with Thermal conductivity of 0.25 - 0.29 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.8 [-] Show Material materials with Dielectric constant of 2.8 [-] |
3.2 [-] Show Material materials with Dielectric constant of 3.2 [-] | |
Electrical resistivity | 10000000000000.0 - 500000000000000.0 Ω·m Show Material materials with Electrical resistivity of 10000000000000.0 - 500000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Dental implants, electronic couplings, orthopedic implants, medical microtubes, USB sticks | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion, coating, blow molding, thermoforming, laser sintering, compression molding |