General
Property | Value |
---|---|
Density | 1.3 - 1.32 g/cm³ Show Material materials with Density of 1.3 - 1.32 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 3.7 - 4.3 GPa Show Material materials with Elastic modulus of 3.7 - 4.3 GPa | ||
Elongation | 10.0 - 35.0 % Show Material materials with Elongation of 10.0 - 35.0 % | ||
Impact strength, Charpy notched | 3.8 kJ/m² Show Material materials with Impact strength, Charpy notched of 3.8 kJ/m² | ||
Tensile strength | 100.0 - 115.0 MPa Show Material materials with Tensile strength of 100.0 - 115.0 MPa | at 10-35% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 4.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 4.5e-05 1/K |
Melting point | 365.0 - 375.0 °C Show Material materials with Melting point of 365.0 - 375.0 °C |
Specific heat capacity | 2200 J/(kg·K) Show Material materials with Specific heat capacity of 2200 J/(kg·K) |
Thermal conductivity | 0.21 - 0.29 W/(m·K) Show Material materials with Thermal conductivity of 0.21 - 0.29 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 3.4 [-] Show Material materials with Dielectric constant of 3.4 [-] |
3.5 [-] Show Material materials with Dielectric constant of 3.5 [-] | |
Electrical resistivity | 10000000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 10000000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Gears, conveyor elements, bearings | |
Processing methods | Injection molding, extrusion, compression molding |