Polysulfone Reinforced with 30% Glass Fibre (PSU+GF30)

Alternative and trade names
It is a 30% glass reinforced, medium viscosity injection molding PESU grade. It exhibits high rigidity & strength, outstanding thermal stability, creep strength at high temperatures, resistance to fracture, superheated steam, oil, fuel, fluorine & coolants, good toughness & impact-resistance, high stiffness, good dielectric properties, high mechanical strength, very good fire behavior, excellent hydrolysis resistance, high resistance to thermal aging, very high long-term service temperature, resistance to weathering, good dimensional stability and good electrical insulating capacity.
Want to keep this datasheet? Save it now in your required format

Description

It is a 30% glass reinforced engineering polymer (Polysulfone) with medium viscosity injection molding PSU grade, with high rigidity and strength.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.44 - 1.49 g/cm³

Show Material materials with Density of 1.44 - 1.49 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

7.4 - 9.5 GPa

Show Material materials with Elastic modulus of 7.4 - 9.5 GPa

Elongation

2.0 - 3.0 %

Show Material materials with Elongation of 2.0 - 3.0 %

Impact strength, Charpy notched

6.0 - 8.5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6.0 - 8.5 kJ/m²

Impact strength, Charpy unnotched

28 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 28 kJ/m²

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

Tensile strength

110.0 - 125.0 MPa

Show Material materials with Tensile strength of 110.0 - 125.0 MPa

at 2-3% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1.9e-05 - 2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.9e-05 - 2e-05 1/K

Thermal conductivity

0.32 W/(m·K)

Show Material materials with Thermal conductivity of 0.32 W/(m·K)

Flammability

UL 94 V1-V0

Electrical

PropertyValue

Dielectric constant

3.5 [-]

Show Material materials with Dielectric constant of 3.5 [-]

3.7 [-]

Show Material materials with Dielectric constant of 3.7 [-]

Electrical resistivity

100000000000000 Ω·m

Show Material materials with Electrical resistivity of 100000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

circuit braker parts, lamp holders, heat shields, impellers, printer cartridges

Fillers

30% Glass Fiber

Processing methods

Injection molding, extrusion