Ethylene Ethyl Acrylate Copolymer (EEA)

Alternative and trade names
Amplify™
Want to keep this datasheet? Save it now in your required format

Description

Polymers offering improved low temperature toughness, high thermal stability, exceptional adhesion to a variety of surfaces, easy processing and melt indices well-suited for multi-layer structures, exceptional compounding versatility and processability, performs well across wide temperature range, excellent elasticity, exceptional performance differentiation and excellent strength.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

0.930 g/cm³

Show Material materials with Density of 0.930 g/cm³

Mechanical

PropertyValueComment

Elongation

700.0 - 750.0 %

Show Material materials with Elongation of 700.0 - 750.0 %

Tensile strength

2.6 - 15.0 MPa

Show Material materials with Tensile strength of 2.6 - 15.0 MPa

at 8-11% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.000200 1/K

Show Material materials with Coefficient of thermal expansion of 0.000200 1/K

Melting point

95.0 - 99.0 °C

Show Material materials with Melting point of 95.0 - 99.0 °C

Thermal conductivity

0.42 W/(m·K)

Show Material materials with Thermal conductivity of 0.42 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

2.7 [-]

Show Material materials with Dielectric constant of 2.7 [-]

Electrical resistivity

100000000000000 Ω·m

Show Material materials with Electrical resistivity of 100000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

high performance packaging, exhaust lines, rollers, protection strips, cord edges

Processing methods

Injection molding, extrusion