Polyamide PA6-3-T (PA NDT/INDT)

Alternative and trade names
Trogamid®
Want to keep this datasheet? Save it now in your required format

Description

Its key features include:


  • Permanent transparency
  • High chemical resistance, very good stress-cracking resistance
  • High mechanical strength
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.120 g/cm³

    Show Material materials with Density of 1.120 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    2.7 - 3.0 GPa

    Show Material materials with Elastic modulus of 2.7 - 3.0 GPa

    Elongation

    40.0 - 70.0 %

    Show Material materials with Elongation of 40.0 - 70.0 %

    Impact strength, Charpy notched

    10.0 - 13.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 10.0 - 13.0 kJ/m²

    Tensile strength

    60.0 - 90.0 MPa

    Show Material materials with Tensile strength of 60.0 - 90.0 MPa

    at 7-8% strain

    Impact strength, Charpy unnotched

    no break

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    5e-05 - 8e-05 1/K

    Show Material materials with Coefficient of thermal expansion of 5e-05 - 8e-05 1/K

    Melting point

    250.0 - 255.0 °C

    Show Material materials with Melting point of 250.0 - 255.0 °C

    Specific heat capacity

    1450.0 - 1600.0 J/(kg·K)

    Show Material materials with Specific heat capacity of 1450.0 - 1600.0 J/(kg·K)

    Thermal conductivity

    0.21 - 0.23 W/(m·K)

    Show Material materials with Thermal conductivity of 0.21 - 0.23 W/(m·K)

    Flammability

    UL 94 HB-V2

    Electrical

    PropertyValue

    Dielectric constant

    3 [-]

    Show Material materials with Dielectric constant of 3 [-]

    4.6 [-]

    Show Material materials with Dielectric constant of 4.6 [-]

    Electrical resistivity

    100000000000.0 - 10000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 100000000000.0 - 10000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    pressure sensor bells, flow meters, medical equipment

    Processing methods

    Injection molding, extrusion, blow molding