Description

PFA has exceptional heat resistance, excellent electrical properties and excellent chemical and weather resistance. Available in both FLEX and ultra high purity (UHP) grades, PFA is the material of choice for semiconductor manufacturing.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

2.12 - 2.17 g/cm³

Show Material materials with Density of 2.12 - 2.17 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

0.6 - 0.7 GPa

Show Material materials with Elastic modulus of 0.6 - 0.7 GPa

Elongation

300 %

Show Material materials with Elongation of 300 %

Tensile strength

20.0 - 35.0 MPa

Show Material materials with Tensile strength of 20.0 - 35.0 MPa

at 300% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.0001 - 0.00016 1/K

Show Material materials with Coefficient of thermal expansion of 0.0001 - 0.00016 1/K

Melting point

305.0 - 310.0 °C

Show Material materials with Melting point of 305.0 - 310.0 °C

Specific heat capacity

1080 J/(kg·K)

Show Material materials with Specific heat capacity of 1080 J/(kg·K)

Thermal conductivity

0.19 - 0.26 W/(m·K)

Show Material materials with Thermal conductivity of 0.19 - 0.26 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

2 [-]

Show Material materials with Dielectric constant of 2 [-]

2.1 [-]

Show Material materials with Dielectric constant of 2.1 [-]

Electrical resistivity

10000000000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

cable insulation, heat-sealing adhesives, chimney linings

Processing methods

Injection molding, extrusion, compression molding, blow molding, coating