Ethylene chlorotrifluoroethylene (ECTFE)

Alternative and trade names
Halar®
Want to keep this datasheet? Save it now in your required format

Description

It is a partially fluorinated semi-crystalline polymer offering a unique combination of properties for highly demanding industries. It is widely used in anti-corrosion applications as a lining or in self-supporting constructions (piping). Its excellent fire resistance properties and chemical resistance make it a first choice in wire and cable applications. It offers purity, surface smoothness, chemical resistance and fire resistance which are key characteristics in the semiconductor and photovoltaic markets.Key Features:


  • Low permeability
  • Excellent weatherability
  • High purity
  • Excellent release properties
  • Good abrasion resistance
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.68 - 1.7 g/cm³

    Show Material materials with Density of 1.68 - 1.7 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    1.4 - 1.7 GPa

    Show Material materials with Elastic modulus of 1.4 - 1.7 GPa

    Elongation

    150.0 - 450.0 %

    Show Material materials with Elongation of 150.0 - 450.0 %

    Tensile strength

    28.0 - 31.0 MPa

    Show Material materials with Tensile strength of 28.0 - 31.0 MPa

    at 5% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    7e-05 - 0.0001 1/K

    Show Material materials with Coefficient of thermal expansion of 7e-05 - 0.0001 1/K

    Melting point

    225.0 - 242.0 °C

    Show Material materials with Melting point of 225.0 - 242.0 °C

    Specific heat capacity

    1000 J/(kg·K)

    Show Material materials with Specific heat capacity of 1000 J/(kg·K)

    Thermal conductivity

    0.14 - 0.18 W/(m·K)

    Show Material materials with Thermal conductivity of 0.14 - 0.18 W/(m·K)

    Flammability

    UL 94 V0

    Electrical

    PropertyValue

    Dielectric constant

    2.3 [-]

    Show Material materials with Dielectric constant of 2.3 [-]

    2.6 [-]

    Show Material materials with Dielectric constant of 2.6 [-]

    Electrical resistivity

    10000000000000 Ω·m

    Show Material materials with Electrical resistivity of 10000000000000 Ω·m

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    cable sheathing, radio chemistry, chemical containers, fibers for fire-resistant upholstery

    Processing methods

    Injection molding, extrusion, coating