Methacrylate-butadiene-styrene (MBS)

Alternative and trade names
Zylar®
Want to keep this datasheet? Save it now in your required format

Description

Clear impact modified styrene acrylic copolymers offer practical toughness, excellent clarity and superior processing over competitive materials such as polycarbonate and copolyesters. In spiral flow tests, Zylar resins flow the same distance as polycarbonate at significantly lower temperatures. This leads to higher productivity, lower energy consumption and less molded-in stress.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.01 - 1.11 g/cm³

Show Material materials with Density of 1.01 - 1.11 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

1.6 - 2.4 GPa

Show Material materials with Elastic modulus of 1.6 - 2.4 GPa

Elongation

30.0 - 50.0 %

Show Material materials with Elongation of 30.0 - 50.0 %

Impact strength, Charpy notched

4.0 - 12.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 4.0 - 12.0 kJ/m²

Impact strength, Charpy unnotched

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

Tensile strength

21.0 - 55.0 MPa

Show Material materials with Tensile strength of 21.0 - 55.0 MPa

at 2-6% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.000090 1/K

Show Material materials with Coefficient of thermal expansion of 0.000090 1/K

Thermal conductivity

0.17 W/(m·K)

Show Material materials with Thermal conductivity of 0.17 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

2.5 [-]

Show Material materials with Dielectric constant of 2.5 [-]

3.21 [-]

Show Material materials with Dielectric constant of 3.21 [-]

Electrical resistivity

10000000000000 Ω·m

Show Material materials with Electrical resistivity of 10000000000000 Ω·m

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

office accessories, medical devices, displays, cosmetic bottles

Processing methods

Injection molding, extrusion, thermoforming