Polyetherimide Reinforced with 30% Glass Fibre (PEI+GF30)

Alternative and trade names
Ultem™
Want to keep this datasheet? Save it now in your required format

Description

Reinforced engineering polymer (Polyetherimide) with 30% glass fiber. Amorphous thermoplastic polyetherimide (PEI) resins offers outstanding elevated thermal resistance, high strength and stiffness, and broad chemical resistance. They are available in transparent and opaque custom colors. These copolymers are available for even higher heat, chemical and elasticity needs.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.49 - 1.51 g/cm³

Show Material materials with Density of 1.49 - 1.51 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

9.0 - 11.0 GPa

Show Material materials with Elastic modulus of 9.0 - 11.0 GPa

Elongation

2.0 - 3.0 %

Show Material materials with Elongation of 2.0 - 3.0 %

Impact strength, Charpy notched

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

Impact strength, Charpy unnotched

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

Tensile strength

150.0 - 165.0 MPa

Show Material materials with Tensile strength of 150.0 - 165.0 MPa

at 2-3% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2e-05 - 6e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 6e-05 1/K

Thermal conductivity

0.29 W/(m·K)

Show Material materials with Thermal conductivity of 0.29 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

3.3 [-]

Show Material materials with Dielectric constant of 3.3 [-]

3.9 [-]

Show Material materials with Dielectric constant of 3.9 [-]

Electrical resistivity

100000000000000.0 - 1000000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 100000000000000.0 - 1000000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Fillers

30% Glass Fiber

Processing methods

Injection molding