Description

Its key features include:


  • excellent transmission and clarity
  • Very high mechanical strength and rigidity
  • Good weather resistance
  • High stability of the optical characteristics at long-lasting thermal load.
  • Highest heat deflection temperature under load.
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.21 - 1.22 g/cm³

    Show Material materials with Density of 1.21 - 1.22 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    4.0 - 4.1 GPa

    Show Material materials with Elastic modulus of 4.0 - 4.1 GPa

    Elongation

    3 %

    Show Material materials with Elongation of 3 %

    Impact strength, Charpy notched

    1.4 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 1.4 kJ/m²

    Impact strength, Charpy unnotched

    20 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

    Tensile strength

    80.0 - 90.0 MPa

    Show Material materials with Tensile strength of 80.0 - 90.0 MPa

    at 3% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    4.5e-05 - 8e-05 1/K

    Show Material materials with Coefficient of thermal expansion of 4.5e-05 - 8e-05 1/K

    Flammability

    UL 94 HB

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    automotive head- and rear lights, optical fibres, sun roofs, packaging for cosmetics

    Processing methods

    Injection molding, extrusion