Polyamide 1010 (PA1010)

Alternative and trade names
Vestamid®, Rilsan®, Grilamid®, Zytel®,
Want to keep this datasheet? Save it now in your required format

Description

It is an unreinforced, toughened, plasticized, and heat stabilized, biobased polyamide 1010 resin for extrusion.Its key features are:


  • Very low water absorption
  • Very good dimensional stability
  • High resistance to chemicals and weathering
  • Low density
  • Direct organic alternative to PA12
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.04 - 1.07 g/cm³

    Show Material materials with Density of 1.04 - 1.07 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    0.6 - 1.7 GPa

    Show Material materials with Elastic modulus of 0.6 - 1.7 GPa

    Elongation

    220 %

    Show Material materials with Elongation of 220 %

    Impact strength, Charpy notched

    5 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

    no break

    Tensile strength

    33.0 - 55.0 MPa

    Show Material materials with Tensile strength of 33.0 - 55.0 MPa

    at 5-39% strain

    Thermal

    PropertyValueComment

    Coefficient of thermal expansion

    8e-05 - 0.00017 1/K

    Show Material materials with Coefficient of thermal expansion of 8e-05 - 0.00017 1/K

    Max service temperature

    90 °C

    Show Material materials with Max service temperature of 90 °C

    Short

    60.0 - 80.0 °C

    Show Material materials with Max service temperature of 60.0 - 80.0 °C

    Long

    Melting point

    194.0 - 202.0 °C

    Show Material materials with Melting point of 194.0 - 202.0 °C

    Flammability

    UL 94 HB

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    Cell phones, connectors, eyeglass frames, fuel lines

    Other

    You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

    Polymer Advanced Search

    Processing methods

    Injection molding, extrusion