Ethylene Tetrafluoroethylene Reinforced with 25% Glass Fibre (ETFE+GF25)

Alternative and trade names
Tecaflon™
Want to keep this datasheet? Save it now in your required format

Description

Reinforced Ethylene Tetrafluoroethylene (ETFE) with 25% glass fiber.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.86 g/cm³

Show Material materials with Density of 1.86 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

8.2 - 8.4 GPa

Show Material materials with Elastic modulus of 8.2 - 8.4 GPa

Elongation

8.0 - 9.0 %

Show Material materials with Elongation of 8.0 - 9.0 %

Tensile strength

80.0 - 85.0 MPa

Show Material materials with Tensile strength of 80.0 - 85.0 MPa

at 8-9% strain

Thermal

PropertyValue

Coefficient of thermal expansion

1.7e-05 - 3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.7e-05 - 3e-05 1/K

Melting point

270 °C

Show Material materials with Melting point of 270 °C

Specific heat capacity

1950 J/(kg·K)

Show Material materials with Specific heat capacity of 1950 J/(kg·K)

Thermal conductivity

0.21 W/(m·K)

Show Material materials with Thermal conductivity of 0.21 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

2.8 [-]

Show Material materials with Dielectric constant of 2.8 [-]

3.4 [-]

Show Material materials with Dielectric constant of 3.4 [-]

Electrical resistivity

100000000000000 Ω·m

Show Material materials with Electrical resistivity of 100000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Piping elements, saelings, flanges, rollers

Fillers

25% Glass Fiber

Processing methods

Extrusion