Polyetherketoneetherketoneketone (PEKEKK)

Alternative and trade names
Victrex™
Want to keep this datasheet? Save it now in your required format

Description

High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding/extrusion, standard/low flow, colour natural/beige.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.3 - 1.32 g/cm³

Show Material materials with Density of 1.3 - 1.32 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

4.0 - 4.3 GPa

Show Material materials with Elastic modulus of 4.0 - 4.3 GPa

Elongation

10.0 - 30.0 %

Show Material materials with Elongation of 10.0 - 30.0 %

Impact strength, Charpy notched

4 kJ/m²

Show Material materials with Impact strength, Charpy notched of 4 kJ/m²

Tensile strength

110.0 - 115.0 MPa

Show Material materials with Tensile strength of 110.0 - 115.0 MPa

at 10-30% strain

Impact strength, Charpy unnotched

no break

Thermal

PropertyValue

Coefficient of thermal expansion

4.1e-05 - 5.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 4.1e-05 - 5.5e-05 1/K

Melting point

381.0 - 387.0 °C

Show Material materials with Melting point of 381.0 - 387.0 °C

Specific heat capacity

1400 J/(kg·K)

Show Material materials with Specific heat capacity of 1400 J/(kg·K)

Thermal conductivity

0.22 - 0.32 W/(m·K)

Show Material materials with Thermal conductivity of 0.22 - 0.32 W/(m·K)

Flammability

UL 94 V0

Electrical

PropertyValue

Dielectric constant

3 [-]

Show Material materials with Dielectric constant of 3 [-]

Electrical resistivity

100000000000000 Ω·m

Show Material materials with Electrical resistivity of 100000000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Turbocharger impellors, gears, sockets

Processing methods

Injection molding, extrusion