General
Property | Value |
---|---|
Density | 1.3 - 1.32 g/cm³ Show Material materials with Density of 1.3 - 1.32 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 4.0 - 4.3 GPa Show Material materials with Elastic modulus of 4.0 - 4.3 GPa | ||
Elongation | 10.0 - 30.0 % Show Material materials with Elongation of 10.0 - 30.0 % | ||
Impact strength, Charpy notched | 4 kJ/m² Show Material materials with Impact strength, Charpy notched of 4 kJ/m² | ||
Tensile strength | 110.0 - 115.0 MPa Show Material materials with Tensile strength of 110.0 - 115.0 MPa | at 10-30% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 4.1e-05 - 5.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 4.1e-05 - 5.5e-05 1/K |
Melting point | 381.0 - 387.0 °C Show Material materials with Melting point of 381.0 - 387.0 °C |
Specific heat capacity | 1400 J/(kg·K) Show Material materials with Specific heat capacity of 1400 J/(kg·K) |
Thermal conductivity | 0.22 - 0.32 W/(m·K) Show Material materials with Thermal conductivity of 0.22 - 0.32 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 3 [-] Show Material materials with Dielectric constant of 3 [-] |
Electrical resistivity | 100000000000000 Ω·m Show Material materials with Electrical resistivity of 100000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Turbocharger impellors, gears, sockets | |
Processing methods | Injection molding, extrusion |