Reinforced Polyamide 66 with 15% glass fiber,These materials are distinguished by high mechanical strength, hardness, rigidity, thermostability and resistance to hot lubricants and hot water. Parts made from them show dimensional stability and high creep strength.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.2 - 1.26 g/cm³

Show Material materials with Density of 1.2 - 1.26 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

3.5 - 4.5 GPa

Show Material materials with Elastic modulus of 3.5 - 4.5 GPa

Elongation

3.0 - 12.0 %

Show Material materials with Elongation of 3.0 - 12.0 %

Impact strength, Charpy notched

5.0 - 25.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.0 - 25.0 kJ/m²

Impact strength, Charpy unnotched

35 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 35 kJ/m²

95 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 95 kJ/m²

Tensile strength

60.0 - 130.0 MPa

Show Material materials with Tensile strength of 60.0 - 130.0 MPa

at 3-12% strain

Thermal

PropertyValue

Coefficient of thermal expansion

3e-05 - 0.0001 1/K

Show Material materials with Coefficient of thermal expansion of 3e-05 - 0.0001 1/K

Melting point

255.0 - 265.0 °C

Show Material materials with Melting point of 255.0 - 265.0 °C

Thermal conductivity

0.33 W/(m·K)

Show Material materials with Thermal conductivity of 0.33 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

3.5 [-]

Show Material materials with Dielectric constant of 3.5 [-]

9 [-]

Show Material materials with Dielectric constant of 9 [-]

Electrical resistivity

1000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Housings, electrically insulating parts

Fillers

15% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, blow molding, extrusion