General Reinforced Polyamide 6 (PA6+CF60), UD-Tape

Alternative and trade names
Vestape, Cetex®
.XLSX
.PDF
Save

Description

Reinforced engineering composite with 60% carbon fiber

Properties

General

Density ρ

1.42 - 1.47 g/cm³ at 20 °C

Mechanical

Elastic modulus E

100 - 125 GPa at 20 °C

Elongation A

1.5 % at 20 °C

Max allowed stress σmax

1800 - 2000 MPa at 20 °C

at 1.5% strain

Thermal

Melting point Tm

220 °C

Optical

Transparency

no

Technological properties

Application areas

Lightweight car body, structural components, sporting goods, under hood applications, housings

Fillers

60% Carbon Fibers

Processing methods

Thermoforming, back injection molding, insert moulding

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.