Polypropylene Reinforced with 70% Glass Fibers(PP+GF70), UD-Tape

Alternative and trade names
Udmax™
Want to keep this datasheet? Save it now in your required format

Description

Reinforced polypropylene PP with 70% glass fiber with high strength and stiffness, excellent processability & corrosion and fatigue resistance.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.650 g/cm³

Show Material materials with Density of 1.650 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

37 GPa

Show Material materials with Elastic modulus of 37 GPa

Elongation

2.6 %

Show Material materials with Elongation of 2.6 %

Tensile strength

948 MPa

Show Material materials with Tensile strength of 948 MPa

at 2.6% strain

Thermal

PropertyValue

Melting point

163 °C

Show Material materials with Melting point of 163 °C

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Truck bodies, vehicles, vehicle enclosures

Fillers

70% Glass Fiber

Processing methods

Thermoforming