Polyamide 1012 (PA1012)

Alternative and trade names
Vestamid®
Want to keep this datasheet? Save it now in your required format

Description

It is an unmodified, easy-flowing, tough-improved PA 1012 resin for injection molding or modification by a compounding process. Due to its semi-crystalline morphology it provides an excellent chemical resistance, e.g., against greases, oils, fuels and hydraulic fluids. It is also medium viscosity, easy-flowing.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.03 - 1.05 g/cm³

Show Material materials with Density of 1.03 - 1.05 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

1.3 GPa

Show Material materials with Elastic modulus of 1.3 GPa

Impact strength, Charpy notched

12.0 - 24.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 12.0 - 24.0 kJ/m²

Tensile strength

40 MPa

Show Material materials with Tensile strength of 40 MPa

at 5% strain

Thermal

PropertyValue

Melting point

190 °C

Show Material materials with Melting point of 190 °C

Flammability

UL 94 HB-V2

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

Writing utensils, electronic components, winter sport equipment, mono- and multifilaments, textiles

Processing methods

Injection molding, extrusion, melt spin processes