Poly(phenylene ether) Reinforced with 30% Glass Fibers (PPO+GF30)

Alternative and trade names
Formpoly®, Norfor®
Want to keep this datasheet? Save it now in your required format

Description

It is a multipurpose polyphenylene ether (PPO) resin reinforced with 30% glass fiber. Is a heat stabilized grade exhibiting low odor and low warpage. Offers easy flow, easy molding and good dimensional stability.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.27 - 1.3 g/cm³

Show Material materials with Density of 1.27 - 1.3 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

7.5 - 9.0 GPa

Show Material materials with Elastic modulus of 7.5 - 9.0 GPa

Elongation

1.5 - 3.0 %

Show Material materials with Elongation of 1.5 - 3.0 %

Impact strength, Charpy notched

7.0 - 12.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 7.0 - 12.0 kJ/m²

Impact strength, Charpy unnotched

25 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m²

Tensile strength

100.0 - 110.0 MPa

Show Material materials with Tensile strength of 100.0 - 110.0 MPa

at 1.5-3% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2.5e-05 - 7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.5e-05 - 7e-05 1/K

Thermal conductivity

0.28 W/(m·K)

Show Material materials with Thermal conductivity of 0.28 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

2.9 [-]

Show Material materials with Dielectric constant of 2.9 [-]

3.5 [-]

Show Material materials with Dielectric constant of 3.5 [-]

Electrical resistivity

10000000000000.0 - 300000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 10000000000000.0 - 300000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Pump housings, levers, brackets, connectors

Fillers

30% Glass Fiber

Processing methods

Injection molding