Description

Polypropylene with 50% wood having acoustical barrier properties.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.05 - 1.15 g/cm³

Show Material materials with Density of 1.05 - 1.15 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

3.2 - 5.1 GPa

Show Material materials with Elastic modulus of 3.2 - 5.1 GPa

Elongation

1.5 - 2.5 %

Show Material materials with Elongation of 1.5 - 2.5 %

Impact strength, Charpy notched

4.0 - 5.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 4.0 - 5.0 kJ/m²

Impact strength, Charpy unnotched

10 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 10 kJ/m²

25 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m²

Tensile strength

20.0 - 45.0 MPa

Show Material materials with Tensile strength of 20.0 - 45.0 MPa

at 1.5-2.5% strain

Thermal

PropertyValue

Coefficient of thermal expansion

0.00005 1/K

Show Material materials with Coefficient of thermal expansion of 0.00005 1/K

Thermal conductivity

0.25 - 0.26 W/(m·K)

Show Material materials with Thermal conductivity of 0.25 - 0.26 W/(m·K)

Flammability

UL 94 HB

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Furniture legs, buttons, reels

Fillers

50% Wood Powder