Polyphthalamide Reinforced with 30% Carbon Fibers (PPA+CF30)

Alternative and trade names
OnForce™,Radiflam®, Radilom®
Want to keep this datasheet? Save it now in your required format

Description

Long Fiber Thermoplastic (LFT, PPA with 30% carbon fiber) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.3 - 1.33 g/cm³

Show Material materials with Density of 1.3 - 1.33 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

23.0 - 26.0 GPa

Show Material materials with Elastic modulus of 23.0 - 26.0 GPa

Elongation

1.0 - 2.0 %

Show Material materials with Elongation of 1.0 - 2.0 %

Impact strength, Charpy notched

9.0 - 12.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 9.0 - 12.0 kJ/m²

Impact strength, Charpy unnotched

48 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 48 kJ/m²

55 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 55 kJ/m²

Tensile strength

220.0 - 320.0 MPa

Show Material materials with Tensile strength of 220.0 - 320.0 MPa

at 1-2% strain

Thermal

PropertyValue

Coefficient of thermal expansion

3e-05 - 6e-05 1/K

Show Material materials with Coefficient of thermal expansion of 3e-05 - 6e-05 1/K

Melting point

315 °C

Show Material materials with Melting point of 315 °C

Flammability

UL 94 HB

Electrical

PropertyValue

Electrical resistivity

10000 Ω·m

Show Material materials with Electrical resistivity of 10000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Fuel systems applications, automotive electronics

Fillers

30% Carbon Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding