Polyamide 9T (PA9T)

Alternative and trade names
Genestar™
Want to keep this datasheet? Save it now in your required format

Description

It is a specially designed long-chain polyphthalamide (PPA) that combines a low water absorption and excellent mechanical properties over a broad temperature range. Depending on the grade the key features are: Mechanical properties at high temperature, low water absorption, outstanding fuel barrier, heat resistance, a low friction coefficient, Low wear, chemical resistance, long term heat resistance, high reflectivity, less color change by heat and light, high flowability

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.06 - 1.17 g/cm³

Show Material materials with Density of 1.06 - 1.17 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

1.4 - 2.7 GPa

Show Material materials with Elastic modulus of 1.4 - 2.7 GPa

Elongation

5.0 - 40.0 %

Show Material materials with Elongation of 5.0 - 40.0 %

Impact strength, Charpy notched

5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

no break

Tensile strength

50.0 - 85.0 MPa

Show Material materials with Tensile strength of 50.0 - 85.0 MPa

at 4-7% strain

Impact strength, Charpy unnotched

no break

Thermal

PropertyValue

Coefficient of thermal expansion

5.5e-05 - 7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 5.5e-05 - 7e-05 1/K

Melting point

265.0 - 300.0 °C

Show Material materials with Melting point of 265.0 - 300.0 °C

Specific heat capacity

1400.0 - 1500.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1400.0 - 1500.0 J/(kg·K)

Thermal conductivity

0.24 - 0.25 W/(m·K)

Show Material materials with Thermal conductivity of 0.24 - 0.25 W/(m·K)

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Gears, wheels, retainers for quick connectors, flexible bands, tube applications

Processing methods

Injection molding, extrusion, blow molding