General
Property | Value | Temperature |
---|---|---|
Density | 1.2 - 1.26 g/cm³ Show Material materials with Density of 1.2 - 1.26 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elongation | 200 - 400 % Show Material materials with Elongation of 200 - 400 % at 23.0 °C | 23.0 °C | |
Tensile strength | 20 - 40 MPa Show Material materials with Tensile strength of 20 - 40 MPa at 23.0 °C | 23.0 °C | at 200-400% strain |
Thermal
Property | Value | Temperature |
---|---|---|
Melting point | 110 - 120 °C Show Material materials with Melting point of 110 - 120 °C | |
Specific heat capacity | 1500 J/(kg·K) Show Material materials with Specific heat capacity of 1500 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 0.17 W/(m·K) Show Material materials with Thermal conductivity of 0.17 W/(m·K) at 23.0 °C | 23.0 °C |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Biodegradable packaging, hot beverage cups, cosmetics bottles, bags | |
Processing methods | Injection molding, extrusion, foaming, blow molding |