Polybutylene succinate adipate (PBSA)

Alternative and trade names
Bionolle®
Want to keep this datasheet? Save it now in your required format

Description

Low modulus and fast biodegradability

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.230 g/cm³

Show Material materials with Density of 1.230 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

0.32 - 0.34 GPa

Show Material materials with Elastic modulus of 0.32 - 0.34 GPa

Elongation

700.0 - 1000.0 %

Show Material materials with Elongation of 700.0 - 1000.0 %

Tensile strength

40.0 - 45.0 MPa

Show Material materials with Tensile strength of 40.0 - 45.0 MPa

at 700-1000% strain

Thermal

PropertyValue

Melting point

95 °C

Show Material materials with Melting point of 95 °C

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Biodegradable packaging, films

Processing methods

Extrusion