General
Property | Value | Temperature |
---|---|---|
Density | 1.1 - 1.4 g/cm³ Show Material materials with Density of 1.1 - 1.4 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 0.6 - 3 GPa Show Material materials with Elastic modulus of 0.6 - 3 GPa at 23.0 °C | 23.0 °C | |
Elongation | 1 - 135 % Show Material materials with Elongation of 1 - 135 % at 23.0 °C | 23.0 °C | |
Impact strength, Charpy unnotched | 3 - 15 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 3 - 15 kJ/m² at 23.0 °C | 23.0 °C | |
Tensile strength | 10 - 45 MPa Show Material materials with Tensile strength of 10 - 45 MPa at 23.0 °C | 23.0 °C | at 1-135% strain |
Thermal
Property | Value |
---|---|
Melting point | 135 - 155 °C Show Material materials with Melting point of 135 - 155 °C |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Refuse bags, diapers, foamed trays and boxes, pharmaceutical capsules, biodegradable packaging | |
Processing methods | Injection molding, thermoforming, extrusion, foaming |