Poly-M-Xylylenadipamid (PAMXD6)

Want to keep this datasheet? Save it now in your required format

Description

It is a crystalline polyamide produced by polycondensation of MXDA with adipic acid. Different from Nylon 6 and Nylon 66, Nylon-MXD6 is an aliphatic polyamide containing an aromatic ring in its main chain. Compared with Nylon 6 and Nylon 66, Nylon-MXD6 has the following favorable characteristics:


  • Greater strength and elastic modulus
  • High glass-transition temperature
  • Low water absorption and moisture permeability
  • Favorable crystallization speed and ease of molding and fabrication
  • Excellent gas-barrier properties
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.220 g/cm³

    Show Material materials with Density of 1.220 g/cm³

    Mechanical

    PropertyValue

    Elastic modulus

    4.7 GPa

    Show Material materials with Elastic modulus of 4.7 GPa

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    0.000050 1/K

    Show Material materials with Coefficient of thermal expansion of 0.000050 1/K

    Melting point

    235.0 - 240.0 °C

    Show Material materials with Melting point of 235.0 - 240.0 °C

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    Monofilaments, food packaging, bottles, trays, cups

    Processing methods

    Injection molding, extrusion, blow molding