Acrylonitrile-butadiene-styrene + Polycarbonate (ASA+PC)

Alternative and trade names
Geloy, Luran®
Want to keep this datasheet? Save it now in your required format

Description

PC/ASA blends provide very good UV-Stability and surface properties. They are widely used for exterior parts in automotive applications. This material can be used to avoid the painting process. PC/ASA blends can be used in injection molding including flame retardant applications. Benefits and features:


  • High gloss and matte surfaces
  • High temperature stability
  • Excellent UV stability and high Impact strength at low temperatures
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.11 - 1.16 g/cm³

    Show Material materials with Density of 1.11 - 1.16 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    2.3 - 2.6 GPa

    Show Material materials with Elastic modulus of 2.3 - 2.6 GPa

    Elongation

    25.0 - 180.0 %

    Show Material materials with Elongation of 25.0 - 180.0 %

    Impact strength, Charpy notched

    20.0 - 70.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 20.0 - 70.0 kJ/m²

    Tensile strength

    50.0 - 65.0 MPa

    Show Material materials with Tensile strength of 50.0 - 65.0 MPa

    at 3-7% strain

    Impact strength, Charpy unnotched

    no break

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    6e-05 - 9e-05 1/K

    Show Material materials with Coefficient of thermal expansion of 6e-05 - 9e-05 1/K

    Thermal conductivity

    0.17 - 0.25 W/(m·K)

    Show Material materials with Thermal conductivity of 0.17 - 0.25 W/(m·K)

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    2.8 [-]

    Show Material materials with Dielectric constant of 2.8 [-]

    3.5 [-]

    Show Material materials with Dielectric constant of 3.5 [-]

    Electrical resistivity

    100000000000.0 - 10000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 100000000000.0 - 10000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Radiator grilles, mirror housings, truck cabin parts, wind turbines

    Processing methods

    Injection molding, blow molding, extrusion, thermoforming