Description

Depending on the grade it has the following features:


  • Thermal aging resistance
  • High flow
  • Anti vibration properties
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.09 - 1.13 g/cm³

    Show Material materials with Density of 1.09 - 1.13 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    1.5 - 2.0 GPa

    Show Material materials with Elastic modulus of 1.5 - 2.0 GPa

    Elongation

    70.0 - 110.0 %

    Show Material materials with Elongation of 70.0 - 110.0 %

    Impact strength, Charpy notched

    40.0 - 60.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 40.0 - 60.0 kJ/m²

    Tensile strength

    45.0 - 55.0 MPa

    Show Material materials with Tensile strength of 45.0 - 55.0 MPa

    at 10-20% strain

    Impact strength, Charpy unnotched

    no break

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    6e-05 - 0.00011 1/K

    Show Material materials with Coefficient of thermal expansion of 6e-05 - 0.00011 1/K

    Melting point

    280 °C

    Show Material materials with Melting point of 280 °C

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    3.1 [-]

    Show Material materials with Dielectric constant of 3.1 [-]

    3.4 [-]

    Show Material materials with Dielectric constant of 3.4 [-]

    Electrical resistivity

    20000000000000.0 - 100000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 20000000000000.0 - 100000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Instrument panels, vehicle front ends

    Processing methods