Poly(oxymethylene) Reinforced with 40% Glass Fibers (POM+GF40)

Alternative and trade names
Lucel®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced engineering plastic (Polyoxymethylene) with 40% glass fiber and high Rigidity.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.7 - 1.72 g/cm³

Show Material materials with Density of 1.7 - 1.72 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

12.0 - 13.0 GPa

Show Material materials with Elastic modulus of 12.0 - 13.0 GPa

Elongation

1.5 - 3.0 %

Show Material materials with Elongation of 1.5 - 3.0 %

Impact strength, Charpy notched

5.0 - 10.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.0 - 10.0 kJ/m²

Impact strength, Charpy unnotched

20 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m²

25 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m²

Tensile strength

120.0 - 140.0 MPa

Show Material materials with Tensile strength of 120.0 - 140.0 MPa

at 1.5-3% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2e-05 - 7e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 7e-05 1/K

Melting point

165.0 - 167.0 °C

Show Material materials with Melting point of 165.0 - 167.0 °C

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

4.2 [-]

Show Material materials with Dielectric constant of 4.2 [-]

4.5 [-]

Show Material materials with Dielectric constant of 4.5 [-]

Electrical resistivity

1000000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Casings of pumps, pivot bearings

Fillers

40% Glass Fiber

Processing methods

Injection molding