Description

A copolymer of ethylene and methacrylic acid used as a coating and packaging material. The coating is known for increasing the toughness, aerodynamics, and durability of the surface.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

0.91 - 0.97 g/cm³

Show Material materials with Density of 0.91 - 0.97 g/cm³

Mechanical

PropertyValueComment

Elongation

200.0 - 500.0 %

Show Material materials with Elongation of 200.0 - 500.0 %

Tensile strength

20.0 - 40.0 MPa

Show Material materials with Tensile strength of 20.0 - 40.0 MPa

at 200-500% strain

Thermal

PropertyValue

Melting point

80.0 - 100.0 °C

Show Material materials with Melting point of 80.0 - 100.0 °C

Optical

PropertyValue

Transparency

yes

Technological properties

Property
Application areas

Food packaging, skin packaging, golfballs skins, skiboots

Processing methods