Nickel Molybdenum Steel
ASTM A387 Grade 11 Class 1, Annealed, Normalized and Tempered, or Quenched and TemperedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Alpha-Beta-Legierung
DIN 17851 Grade 3.7185Alpha-Beta-Legierung
DIN 17851 Grade 3.7185Wrought Copper Bronze Aluminium Bronze
AMPCO® 18 Extruded and drawn rounds and rectangular barsGeliefert von:
AMPCO METALLeaded Brass
EN 1652 Grade CuZn39Pb0.5 R340Alpha-Beta-Legierung
DIN 17851 Grade TiAl6V6Sn2 Annealed